Human: The scan was taken with FUEL3D. Printer: Gigabot. Filament: I used 3mm White PLA. Layer Thickness: It was printed at a thickness of .1mm per layer. Orientation: The print began from the top of the head and went down to the chin, done vertically. Support: Yes, support material was used. Bed temp: Initially, the bed temperature was set at 65 degrees Celsius for the first 30 layers before dropping it to 45 degrees Celsius. Hot end: I heated the hot end to a temperature ranging from 190 to 185 degrees Celsius. Print time: The entire print took approximately 28 hours to complete. I ran the printer at half speed to ensure everything went smoothly, and I'm confident that it can be sped up further.